Dynamic assessment of titanium surface oxides following mechanical damage reveals only partial passivation under inflammatory conditions

  • Georgios A. Kotsakis
  • , Li Xie
  • , Danyal A. Siddiqui
  • , Diane Daubert
  • , Daniel J. Graham
  • , Francisco Javier Gil

Research output: Contribution to journal › Article › peer-review

Abstract

Motivated by clinical problems of titanium implant degradation, we developed a workflow that enabled assessment of surface oxide dynamics as a function of clinical interventions and inflammation conditions. We found that mechanical damage led to decrease of stoichiometric TiO2 ratio in the passivation oxide film and further resulted in accelerated degradation under inflammatory anaerobic conditions. This method can be employed for the assessment of surface oxides to monitor implant safety.

Original languageEnglish (US)
Article number98
Journalnpj Materials Degradation
Volume8
Issue number1
DOIs
StatePublished - Dec 2024

ASJC Scopus subject areas

  • Ceramics and Composites
  • Chemistry (miscellaneous)
  • Materials Science (miscellaneous)
  • Materials Chemistry

Fingerprint

Dive into the research topics of 'Dynamic assessment of titanium surface oxides following mechanical damage reveals only partial passivation under inflammatory conditions'. Together they form a unique fingerprint.

Cite this